大阪大学超高圧電子顕微鏡センター関係発表論文リスト2003年度

   | 2008 年 |   | 2007 年 |   | 2006 年 |   | 2005 年 |   | 2004 年 |   | 2003 年 |   | 2002 年 |




1. In Situ HREM Study on the Structural Instability of Isolated Nanometer-sized Particles in the Sn-Bi
  system

      J. G. Lee and H. Mori
      Journal of Electron Microscopy. Vol. 52, No. 1 (2003) 57-62.

2. Particle-size Dependence of Alloy Phase Formation in Isolated Particles in the In-Sn System
      J. G. Lee and H. Mori
      J. V. Sci. Technol. A. Vol. 21, No. 1 (2003) 32-36.

3. 人に優しい医療用セラミック被覆穿刺針の開発
      森 博太郎、井口 征夫、福田 浩之、江原 正明
      まてりあ 第42巻 第2号 (2003) 151-153.

4. Interfacial Microstructure between Sn-3Ag-xBi Alloy and Cu Substrate with or without Electrolytic
  Ni Plating

      C. W. Hwang, J. G. Lee, K. Suganuma, and H. Mori
      Journal of Electronic Materials, Vol.32, No.2 (2003) 52.

5. Interface Microstructure between Fe-42Ni Alloy and Pure Sn
      C. W. Hwang, K. Suganuma, J. G. Lee, and H. Mori
      J. Mater. Res., Vol.18, No.5 (2003) 1.

6. Sn-Ag 系はんだと無電解 Ni-P 合金めっきとの界面反応と強度
      上西 啓介、小原 泰浩、酒谷 茂昭、小林 絋二郎
      9th Symposium on “Microjoining and Assembly Technology in Electronics”
       Febraury 6-7, 2003, Yokohama, 289-294.

7. Real-Time Scanning Tunneling Microscope Observation of High-Temperature Oxygen Reaction with
  the 6H-SiC(0001) √3x√3Surface

      H. Okado, O.Kubo, N.Yamaoka, S.Itou, A. Nishida, M. Katayama, and K.Oura
      Jpn. J. Appl. Phys. Vol. 42 (2003) L451-454.

8. Thermally Stable Amorphous Phase in Nanometer-Sized Alloy Particles
      J. G. Lee, H. Mori
      Journal of Metastable and Nanocrystalline Vols.15-16 (2003) 427-432.

9. Microstructure and properties of ecoceramics /metal composites with interpenetrating
  Networks
      Z. Di, X. Xian-qing, F. Tong-xiang, S. Bing-he, T. Sakata, H. Mori, and T. Okabe
      Materials Science and Engineering A. 351 (2003) 109-116.

10. Alloy Phase Formation in Isolated Nanometer-sized Particles in the Au-Sn and Sn-Bi Systems
      J-G. Lee, H. Mori, and H. Yasuda
      Mat. Res. Soc. Symp. Proc. Vol. 754 c 2003 Materials Research Society.

11. Interface microstructure between Fe-42Ni alloy and pure Sn
      C-H. Hwang and K. Suganuma, J-G. Lee, and H. Mori
      Materials Research Society Volume 18, Number 5 May 2003.

12. Comparison among the formation processes of extended defects in Si under irradiation with
  low-energy H+, He+ions and high-energy electorns

      K. Arakawa, K. Saitoh, H. Mori, and K. Ono
      Nuclear Instruments and Methods in Physics Research B. 206 (2003) 76-80.

13. In situ observation of oxygen-induced anisoropic surface etching processes at 6H-SiC(0001) by
  variable temperature scanning tunneling microscope

      H. Okado, O. Kubo, N. Yamaoka, S. Itou, M. Katayama, and K. Oura
      Applied Surface Science 212-213 (2003) 575-578.

14. Field Emission from Bamboo-Like Multiwalled Caron Nanotube Arrays Enhanced by Mild Oxidation
      M. Matsushima, H. Araki, K. Kamide, T. Sakata, H. Mori, and K. Yoshino
      Jpn. J. Appl. Phys. Vol.42 (2003) L1036-1038.

15. ナノ粒子における合金化反応
      森 博太郎
      シーエムシー出版 2003 年 8 月刊 38-42. 

16. 合金ナノ粒子におけるアモルファス相の形成
      森 博太郎、李 正九
       47 回日本学術会議 材料研究連合講演会 講演論文集 平成 15 年 10 月 29 日(水)、
      30 日(木) 京大会館 129-130.


17. タンパク質複合体の直接観察
      光岡 薫、岩崎 憲治、藤吉 好則
      注目のプロテオミクスの全貌を知る! 第2章 羊土社 103-109.

18. Topology representing network enables highly accurate classification of protein images taken by
  cryo electron-microscope without masking

      T. Ogura, K. Iwasaki, and C. Sato
      Journal of Structural Biology 143 (2003) 185-200.

19. Synthesis of Aligned Carbon Nanofibers at 200℃
      K-Y. Lee, M. Katayama, S. Honda, T. Kuzuoka, T. Miyake, Y. Terao, J-G. Lee, H. Mori, T. Hirao,
      and K. Oura

      The Japan Society of Applied Physics Vol.42 (2003) L804-L806 Part 2, No.7B, 15 July 2003.

20. Insulator-Coated Carbon Nanotubes Synthesized by Pulsed Laser Deposition
      T. Ikuno, M. Katayama, K. Kamada, S. Honda, J-G. Lee, H. Mori, and K. Oura
      The Japan Society of Applied Physics Vol. 42 (2003) L1356-L1358 Part 2, No. 11B, 15
      November 2003.


21. Interface microstructure between 42 alloy and Sn-based lead-free solder
      C.W. Hwang, J.G. Lee, H. Mori, and K. Suganuma
      2003 TMS annual meeting and exhibition Mar. 2-6, 2003, San Diego, CA.

22. In-situ observation of alloy phase formation in nanometer-sized particles in the Sn-Bi system
   [Invited]

      J.G. Lee and H. Mori
      International Symposium on In-situ Electron Microscopy Jan. 20-22, 2003, Nagoya, JAPAN.
      


23. Particle-size Dependence of Crystalline-to-Liquid (C→L) Phase Chage in Nanometer-sized Alloy
  Particles

      J.G. Lee and H. Mori
      10th International Symposium on Metastable, Mechanically Alloyed and Nanocrystalline      
      
Materials (ISMANAM 2003) Foz do Iguacu, Brazil 24-28 August, 2003.


24. Phase change and Morphology in Nanometer-sized Alloy Particles in the Melt plus α-solid Solution,
  Two-phase Region

      J-G. Lee, H. Mori, and H. Yasuda
      1st International Symposium on Active Nano-Characterization and Technology Tsukuba,
      Japan 11-14 November, 2003.


25. Low Temperature Synthesis of Aligned Carbon Nanofibers by Inductively Coupled Plasma Chemical  
  Vapor Deposition

      T. Kazuoka, K-Y. Lee, T. Miyake, Y. Terao, S. Honda, M. Katayama, J-G. Lee, T. Hirao, H. Mori,
      and K. Oura

      The 7th International Conference on Atomically Controlled Surface, Interfaces and
      Nanostructures
Nara. Japan 16-20 November, 2003.

26. Synthesis of high-destiny long carbon nanotubes vertically aligned on metal substrate by thermal
  CVD

      N. Hayashi, K-Y Lee, T. Miyake, S. Honda, M. Katayama, T. Hirao, K. Oura, J-G. Lee, H. Mori,
      K. Endo, M. Kimoto, K. Nishimura, and K. Nishio

      The 7th International Conference on Atomically Controlled Surfaces, Interfaces and
      Nanostructures Nara, Japan 16-20 November, 2003.


27. 原子構造情報を利用したタンパク質の画像解析
      岩崎 憲治、宮澤 淳夫
      電子顕微鏡 Vol. 38 No.3 別刷 2003.


28. TEM Study on Crystalline-to-Liquid Phase Change in Nanometer-sized Alloy Particles
      J-G. Lee and H. Mori
      1st International Symposium on Active Nano-Characterization and Technology
      Nov. 12 (Wed.) - 14 (Fri.), 2003.


29. Doping of magic nanoclusters in the submonolayer In/Si(100) system
      VG. Kotlyar, AV. Zotov, AA. Saranin, EN. Chukurov, TV. Kasyanova, MA. Cherevik,
      IV. Pisarenko, H. Okado, M. Katayama, K. Oura, and VG. Lifshits

      PHYSICAL REVIEW LETTERS 91(2): Art. No. 026104 JUL 11 2003.

30. Phase Separation Induced by Electron Irradiation in GaSb Compound Nanoparticles
      H. Yasuda, H. Mori, and J-G. Lee
      Transactions of the Materials Research of Japan 28 [3] 891-894 (2003).

31. Quantitative analysis of anti-phase boundary tubes in cyclically deformed Fe-40at.% Al single
  crystals by means of magnetic technique

      H. Yasuda, R. Jimba, and Y. Umakoshi
      Scripta Materials 48 (2003) 589-592.

32. Nondestructive evaluation of dislocation structure in cyclically deformed Ni3Fe single crystals using
  magnetic techniques
      H. Yasuda, A. Sasaaki, and Y. Umakoshi
      Journal of Applied Physics, 99[3] (2003),1472-1476.

33. Effect of coherency on interphase boundary sliding in NiAl(β) bicrystals with film-like Ni3Al(γ)
  precipitate along boundary

      T. Sakata, H. Yasuda, and Y. Umakoshi
      Scripta Materials 48 (2003) 749-753.

34. Interphase boundary fracture and grain boundary precipitation of Ni3Al(γ) phase in β-NiAl
  bicrystals

      T. Sakata, H. Yasuda, and Y. Umakoshi
      Acta Materialia 51 (2003) 1561-1572.

35. Controlling factor for nucleation of martensite at grain boundary in Fe-Ni bicrystals
      M. Ueda, H. Yasuda, and Y. Umakoshi
      Acta Materialia 51 (2003) 1007-1017.

36. Orientation Dependence of Pseudoelasticity in Fe3Al Single Crystals
      H. Yasuda, K. Nakano, M. Ueda, and Y. Umakoshi
      Materials Science Forum Vols. 426-432 (2003) pp.1801-1806.

37. Martensitic and Reverse Transformation in Fe-Ni Bicrystals
      M. Ueda, H. Yasuda, and Y. Umakoshi
      Materials Science Forum Vols. 426-432 (2003) pp.1505-1510.

38. Effect of ordering process on giant pseudoelasticity in Fe3Al single crystals
      H. Yasuda, K. Nakano, T. Nakajima, M. Ueda, and Y. Umakoshi
      Acta Materiaalia 51 (2003) 5101-5112.

39. Effect of Antiphase Boundary on tha Pserdoelasticity in Fe3Al Single Crystals
      H. Yasuda, K. Nakano, M. Ueda, and Y. Umakoshi
      Mat. Res. Soc. Symp. Proc. Vol. 753 c 2003 Materials Research Society.

40. Effect of Interphase Boundary Character on Mechanical Properties in NiAl(β) Bicrystals with
  Ni3Al(γ) Precipitates along Grain Boundary

      T. Sakata, H. Yasuda, and Y. Umakoshi
      Mat. Res. Soc. Symp. Proc. Vol. 753 c 2003 Materials Research Society.

41. Observation of Deformation Substructure in Fatigued Intermetallic Alloys Using Magnetic Properties
      Y. Umakoshi and H. Yasuda
      Mat. Res. Soc. Symp. Proc. Vol. 753 c 2003 Materials Research Society.

42. In situ HREM study on the structural instability of isolated nanometer-sized alloy particles in the
  Sn-Bi system

      J-G. Lee and H. Mori
      Journal of Electron Microscopy 52(1): 57-62 (2003).


                      トップページに戻る